This is an old revision of this page, as edited by Chongkian (talk | contribs) at 15:51, 17 October 2023 (stub template should be placed at the very end of article after external link, navbox & category tags per WP:STUBSPACING). The present address (URL) is a permanent link to this revision, which may differ significantly from the current revision.

The handling of the high grade stainless steel joint clips for conical ground glass joints
Plastic joint clips
Plastic joint clips failing due to corrosive and thermal exposure

Joint clips are used to prevent laboratory glassware joints from separating during a reaction process. They are used to secure the two sides together and are available in a variety of materials for different temperature and chemical environments.

Plastic joint clips

Plastic joint clips are usually made of polyacetal, and are colored according to joint sizes. Polyacetal melts at a reasonably low temperature (around 175 °C) and begins to soften around 140 °C. Polyacetal clips suffer another problem in that the material is strongly affected by the corrosive gases.

PTFE joint clips

Polytetrafluoroethylene (PTFE) joint clips are sometimes used, as its recommended temperature peak matches that of most chemistry work. Its highly inert nature also makes it immune to degradation around corrosive gases. However, it is both expensive and will begin producing hydrogen fluoride if heated to beyond its specified temperature. The same is true of using Krytox and chemically resistant Molykote (PTFE thickened, fluoro-based) oils and greases for glassware seals.

Stainless steel joint clips

Stainless steel can withstand the entire temperature spectrum of borosilicate glass and is reasonably inert. Some glassware features barbs (Devil's horns / Viking helmet) sticking out the sides of the tapers. Small stainless steel springs are used on these to hold the joint together. The use of springs is of particular benefit when dealing with positive pressures, as they apply enough force for the glass to operate, but will open the taper if an unexpected excursion occurs.